Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP Copolymer SAXALEN™ PPC344G25 SAX AUSTRIA
--
--
Filler, glass fiber reinforced material, 25%, filler by weight,
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | SAX AUSTRIA/SAXALEN™ PPC344G25 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed,60.0mmSpan | ISO 75-2/A | 124 °C |
| Vicat softening temperature | ISO 306/B120 | 114 °C |
| mechanical properties | Test Condition | Test Method | SAX AUSTRIA/SAXALEN™ PPC344G25 |
|---|---|---|---|
| Bending modulus | ISO 178 | 3800 MPa | |
| bending strength | ISO 178 | 84.0 MPa | |
| Tensile modulus | ISO 527-2/1 | 4500 MPa | |
| Tensile strain | Break | ISO 527-2/5 | 3.0 % |
| tensile strength | Break | ISO 527-2/5 | 52.0 MPa |
| Physical properties | Test Condition | Test Method | SAX AUSTRIA/SAXALEN™ PPC344G25 |
|---|---|---|---|
| density | ISO 1183 | 1.05 g/cm³ | |
| Melt Volume Flow Rate (MVR) | 230°C/2.16kg | ISO 1133 | 23.0 cm³/10min |
| impact performance | Test Condition | Test Method | SAX AUSTRIA/SAXALEN™ PPC344G25 |
|---|---|---|---|
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 11 kJ/m² |
| -30°C | ISO 179/1eA | 9.0 kJ/m² | |
| Impact strength of cantilever beam gap | -30°C | ISO 180/1A | 8.0 kJ/m² |
| 23°C | ISO 180/1A | 11 kJ/m² | |
| Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 40 kJ/m² |
| 23°C | ISO 179/1eU | 42 kJ/m² | |
| Suspended wall beam without notch impact strength | 23°C | ISO 180/1U | 35 kJ/m² |
| -30°C | ISO 180/1U | 34 kJ/m² |