Epoxy Magnobond 111-047 Magnolia Plastics, Inc.
--
Electrical and electronic application fields
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodMagnolia Plastics, Inc./Magnobond 111-047
Shore hardnessShoreAASTM D224035
thermal performanceTest ConditionTest MethodMagnolia Plastics, Inc./Magnobond 111-047
thermal conductivityASTMC1770.084 W/m/K
Electrical performanceTest ConditionTest MethodMagnolia Plastics, Inc./Magnobond 111-047
Dielectric constant1MHzASTM D1503.96
Dielectric strengthASTM D14920 kV/mm
Dissipation factor1MHzASTM D1500.017
Volume resistivityASTM D2572.8E+14 ohms·cm
thermosettingTest ConditionTest MethodMagnolia Plastics, Inc./Magnobond 111-047
stripping time127°C60to120 min
Thermosetting componentsHardener按重量计算的混合比:1.0
Resin按重量计算的混合比:1.0
Pot Life(25°C)5800 min
Thermosetting mixed viscosityASTM D23931600 cP
Physical propertiesTest ConditionTest MethodMagnolia Plastics, Inc./Magnobond 111-047
densityASTM D7921.07 g/cm³
Water absorption rate24hrASTM D5700.51 %