Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 EMLON® 6 EMAS Plastik San.Tic.AS.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | EMAS Plastik San.Tic.AS./EMLON® 6 |
|---|---|---|---|
| Shore hardness | ShoreD | ISO 868 | 75to80 |
| thermal performance | Test Condition | Test Method | EMAS Plastik San.Tic.AS./EMLON® 6 |
|---|---|---|---|
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 70.0 °C |
| Melting temperature | ISO 3146 | 220 °C | |
| Vicat softening temperature | ISO 306/B | 205 °C |
| mechanical properties | Test Condition | Test Method | EMAS Plastik San.Tic.AS./EMLON® 6 |
|---|---|---|---|
| Tensile modulus | ISO 527-2 | 2000to3500 MPa | |
| Tensile strain | Break | ISO 527-2 | >6.0 % |
| tensile strength | Yield | ISO 527-2 | >60.0 MPa |
| Physical properties | Test Condition | Test Method | EMAS Plastik San.Tic.AS./EMLON® 6 |
|---|---|---|---|
| density | ISO 1183 | 1.12to1.14 g/cm³ | |
| Shrinkage rate | 0.80to1.0 % | ||
| Stickiness | ISO 307 | 2.40to3.50 cm³/g |
| impact performance | Test Condition | Test Method | EMAS Plastik San.Tic.AS./EMLON® 6 |
|---|---|---|---|
| Impact strength of cantilever beam gap | ISO 180/1A | >7.0 kJ/m² |