Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| thermal performance | Test Condition | Test Method | LCY TAIWAN/1065A BK |
|---|---|---|---|
| Melting temperature | LCY Method | 150 °C | |
| Brittle temperature | ISO 11357-1/-3 | -65 °C | |
| mechanical properties | Test Condition | Test Method | LCY TAIWAN/1065A BK |
| Permanent compression deformation | 22hr @ 70℃ | ISO 815 | 32 % |
| Shore hardness | Injection成型试片,15sec | ISO 868 | 68 Shore A |
| Tensile stress | 23℃,500mm/min,Break | ISO 37 | 5.5 Mpa |
| tear strength | 23℃,500mm/min | ISO 34-1 | 19 kN/m |
| Tensile stress | 23℃,500mm/min,100%伸长率 | ISO 37 | 2.9 Mpa |
| Permanent compression deformation | 70hr @ 125℃ | ISO 815 | 44 % |
| Tensile strain | 23℃,500mm/min,Break | ISO 37 | 300 % |
| Other performance | Test Condition | Test Method | LCY TAIWAN/1065A BK |
| ozone resistance | ASTM D-1149 | 优 |