Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PP Niplene F20 Soredi S.p.a.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Soredi S.p.a./Niplene F20 |
---|---|---|---|
Impact strength of cantilever beam gap | -20°C,3.20mm | ASTM D256 | 40 J/m |
23°C,3.20mm | ASTM D256 | 60 J/m |
hardness | Test Condition | Test Method | Soredi S.p.a./Niplene F20 |
---|---|---|---|
Rockwell hardness | R级 | ASTM D785 | 105 |
Electrical performance | Test Condition | Test Method | Soredi S.p.a./Niplene F20 |
---|---|---|---|
Volume resistivity | IEC 60093 | 1E+15 ohms·cm | |
dielectric strength | 1.00mm | IEC 60243-1 | 60 kV/mm |
relative permittivity | 1MHz | IEC 60250 | 2.70 |
Surface Resistivity | IEC 60093 | 1E+14 ohms | |
Dissipation Factor | 1MHz | IEC 60250 | 0.0 |
Mechanical properties | Test Condition | Test Method | Soredi S.p.a./Niplene F20 |
---|---|---|---|
elongation | 断裂 | ASTM D638 | 5.0 % |
bending strength | 断裂 | ASTM D790 | 80.0 MPa |
tensile strength | 断裂 | ASTM D638 | 60.0 MPa |
Flexural modulus | ASTM D790 | 4200 MPa |
flammability | Test Condition | Test Method | Soredi S.p.a./Niplene F20 |
---|---|---|---|
Hot filament ignition temperature | 2.0mm | IEC 60695-2-13 | 650 °C |
UL flame retardant rating | 3.2mm | UL 94 | HB |
1.6mm | UL 94 | HB |
physical property | Test Condition | Test Method | Soredi S.p.a./Niplene F20 |
---|---|---|---|
Shrinkage rate | MD | ASTM D955 | 0.40to0.80 % |
melt mass-flow rate | 230°C/2.16kg | ASTM D1238 | 2.0 g/10min |
Water absorption rate | 平衡,23°C,50%RH | ISO 62 | 0.20 % |
density | ASTM D792 | 1.04 g/cm³ | |
Shrinkage rate | TD | ASTM D955 | 0.50to1.0 % |
Thermal performance | Test Condition | Test Method | Soredi S.p.a./Niplene F20 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 144 °C |
vicat | ASTM D15254 | 125 °C | |
Linear coefficient of thermal expansion | MD:23到55°C | ISO 11359-2 | 4E-05 cm/cm/°C |