Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPE P-150B-BK TOYOBO JAPAN
DIAFLORA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Supplementary Information | Test Condition | Test Method | TOYOBO JAPAN/P-150B-BK |
---|---|---|---|
Resilience | JISK6301 | 59.0 |
hardness | Test Condition | Test Method | TOYOBO JAPAN/P-150B-BK |
---|---|---|---|
Shore hardness | 邵氏D | ASTM D2240 | 57 |
邵氏A | JISK6301 | 98 |
Mechanical properties | Test Condition | Test Method | TOYOBO JAPAN/P-150B-BK |
---|---|---|---|
Taber abraser | 1000Cycles | ASTM D1044 | 10.0 mg |
elongation | 断裂 | ASTM D638 | 500 % |
tensile strength | -- | ASTM D638 | 38.0 Mpa |
compressive strength | 10%应变 | ASTM D695 | 19.1 Mpa |
Flexural modulus | ASTM D790 | 289 Mpa | |
tensile strength | 50%应变 | ASTM D638 | 19.6 Mpa |
Electrical performance | Test Condition | Test Method | TOYOBO JAPAN/P-150B-BK |
---|---|---|---|
Volume resistivity | ASTM D257 | 2E+14 ohms·cm | |
dielectric strength | JISK2111 | 30 KV/mm |
flammability | Test Condition | Test Method | TOYOBO JAPAN/P-150B-BK |
---|---|---|---|
UL flame retardant rating | UL 94 | HB |
elastomer | Test Condition | Test Method | TOYOBO JAPAN/P-150B-BK |
---|---|---|---|
compression set | JISK6301 | 60 % | |
tear strength | ASTM D624 | 176 kN/m |
physical property | Test Condition | Test Method | TOYOBO JAPAN/P-150B-BK |
---|---|---|---|
melt mass-flow rate | 230°C/2.16kg | ASTM D1238 | 20 g/10min |
Shrinkage rate | MD:2.00mm | ASTM D955 | 1.3 % |
Water absorption rate | 平衡,23°C,65%RH | ASTM D570 | 0.36 % |
Thermal performance | Test Condition | Test Method | TOYOBO JAPAN/P-150B-BK |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 117 °C |
vicat | ASTM D1525 | 190 °C | |
brittle temperature | JISK6301 | <-65.0 °C | |
melting temperature | DSC | 212 °C | |
Linear coefficient of thermal expansion | MD | ASTME831 | 1.4E-04 cm/cm/°C |