Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPEE KP3340 KOLON KOREA
KOPEL®
--
Flame retardant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Supplementary Information | Test Condition | Test Method | KOLON KOREA/KP3340 |
---|---|---|---|
Resilience | 67 % |
hardness | Test Condition | Test Method | KOLON KOREA/KP3340 |
---|---|---|---|
Shore hardness | ShoreD | ISO 868 | 40 |
ShoreD | ASTM D2240 | 40 |
thermal performance | Test Condition | Test Method | KOLON KOREA/KP3340 |
---|---|---|---|
Brittle temperature | ASTM D746 | <-70.0 °C | |
Hot deformation temperature | 0.45MPa,Unannealed | ASTM D648 | 65.0 °C |
Melting temperature | ASTM D3418 | 170 °C | |
ISO 11357-3 | 180 °C | ||
Vicat softening temperature | ISO 306/A50 | 120 °C |
mechanical properties | Test Condition | Test Method | KOLON KOREA/KP3340 |
---|---|---|---|
Bending modulus | 23°C | ISO 178 | 75.0 Mpa |
23°C | ASTM D790 | 95.1 Mpa | |
elongation | Break,23°C | ASTM D638 | 920 % |
Taber wear resistance | 1000Cycles,CS-17Wheel | ASTM D1044 | 3.00 mg |
Tensile strain | Break,23°C | ISO 527-2 | 800 % |
tensile strength | 23°C | ASTM D638 | 20.6 Mpa |
Yield,23°C | ISO 527-2 | 22.0 Mpa |
Electrical performance | Test Condition | Test Method | KOLON KOREA/KP3340 |
---|---|---|---|
Dielectric constant | ASTM D150 | 4.90 | |
Dielectric strength | IEC 60243-1 | 18 KV/mm | |
Dissipation factor | ASTM D150 | 6E-04 | |
Volume resistivity | IEC 60093 | 1E+15 ohms·cm |
Physical properties | Test Condition | Test Method | KOLON KOREA/KP3340 |
---|---|---|---|
melt mass-flow rate | 200°C/2.16kg | ISO 1133 | 16 g/10min |
200°C/2.16kg | ASTM D1238 | 17 g/10min | |
Shrinkage rate | MD | ISO 294-4 | 1.1 % |
MD | ASTM D955 | 1.1 % | |
TD | ISO 294-4 | 0.94 % | |
Water absorption rate | 23°C,24hr | ISO 62 | 0.65 % |
Equilibrium,23°C,60%RH | ASTM D570 | 0.70 % |
flammability | Test Condition | Test Method | KOLON KOREA/KP3340 |
---|---|---|---|
UL flame retardant rating | 0.8mm | UL 94 | HB |