TPU A 92 P 4637 HUNTSMAN GERMANY
IROGRAN®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | HUNTSMAN GERMANY/A 92 P 4637 |
---|---|---|---|
Shore hardness | ShoreA,Injection | ASTM D2240 | 92 |
ShoreA,Injection | ISO 868 | 92 | |
ShoreD,Injection | ISO 868 | 39 | |
ShoreD,Injection | ASTM D2240 | 39 |
mechanical properties | Test Condition | Test Method | HUNTSMAN GERMANY/A 92 P 4637 |
---|---|---|---|
Wear resistance | ISO 4649 | 30 mm³ |
Physical properties | Test Condition | Test Method | HUNTSMAN GERMANY/A 92 P 4637 |
---|---|---|---|
Melt Volume Flow Rate (MVR) | 190°C/21.6kg | 55.0 cm3/10min | |
Shrinkage rate | 0.90 % | ||
MD | ASTM D955 | 0.40 % |
elastomer | Test Condition | Test Method | HUNTSMAN GERMANY/A 92 P 4637 |
---|---|---|---|
elongation | Break | ASTM D412 | 670 % |
Break | DIN 53504 | 600 % | |
Permanent compression deformation | 23°C,24hr | ASTM D395 | 25 % |
70°C,24hr | ISO 815 | 41 % | |
巴肖氏弹性 | ISO 815 | 34 % | |
70°C,24hr | ASTM D395 | 41 % | |
23°C,24hr | ISO 815 | 25 % | |
tear strength | ISO 34-1 | 74 kN/m | |
ASTM D624 | 116 kN/m | ||
tensile strength | 300%Strain | DIN 53504 | 15.9 Mpa |
300%Strain | ASTM D412 | 14.1 Mpa | |
Break | ASTM D412 | 33.6 Mpa | |
Break | DIN 53504 | 45.0 Mpa | |
100%Strain | ASTM D412 | 8.96 Mpa | |
100%Strain | DIN 53504 | 9.10 Mpa |