plas
Log In

Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PP Copolymer 5C11130 4Plas
--
--
Filler, talc filler, 30%, filler by weight,
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

thermal performanceTest ConditionTest Method4Plas/ 5C11130
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B108 °C
Melting temperatureISO 11357165 °C
Vicat softening temperatureISO 306/B68.0 °C
mechanical propertiesTest ConditionTest Method4Plas/ 5C11130
Tensile modulus23°CISO 527-2/52800 MPa
Tensile strainBreak,23°CISO 527-2/515 %
tensile strengthBreak,23°CISO 527-2/525.0 MPa
Electrical performanceTest ConditionTest Method4Plas/ 5C11130
Compared to the anti leakage trace indexIEC 60112PLC 1
Physical propertiesTest ConditionTest Method4Plas/ 5C11130
densityISO 11831.13 g/cm³
melt mass-flow rate230°C/2.16kgISO 11338.0to12 g/10min
Water absorption rateEquilibrium,23°C,50%RHISO 620.050 %
water contentISO 960<1000 ppm
impact performanceTest ConditionTest Method4Plas/ 5C11130
Impact strength of cantilever beam gap-30°CISO 180/1A4.0 kJ/m²
23°CISO 180/1A8.0 kJ/m²
flammabilityTest ConditionTest Method4Plas/ 5C11130
Hot filament ignition temperature2.00mmIEC 60695-2-13650 °C