plas
Log In

Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PUR-Capro/MDI C900 CHEMTURU USA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodCHEMTURU USA/ C900
Shore hardnessShoreA2ASTM D224086to89
ShoreA3ASTM D224087to89
Supplementary InformationTest ConditionTest MethodCHEMTURU USA/ C900
Wear factorDIN2592
DIN3890
NBS21300 %
NBS31700 %
filmTest ConditionTest MethodCHEMTURU USA/ C900
Tear resistance of pants type--2ASTM D193833.3 N/mm
--3ASTM D193842.7 N/mm
mechanical propertiesTest ConditionTest MethodCHEMTURU USA/ C900
Wear factor--3,相对体积损失17.0 mm³
--2,相对体积损失25.0 mm³
thermosettingTest ConditionTest MethodCHEMTURU USA/ C900
Post curing time120°C516to24 hr
140°C616to24 hr
storage stability70°C120 min
50°C1400 min
stripping time140°C10 min
120°C20 min
Physical propertiesTest ConditionTest MethodCHEMTURU USA/ C900
densityASTM D7921.13 g/cm³
elastomerTest ConditionTest MethodCHEMTURU USA/ C900
Dart impact--364 %
--264 %
elongationBreak3ASTM D412570 %
Break2ASTM D412540 %
Permanent compression deformation100°C,22hr2ASTM D395B54 %
100°C,22hr3ASTM D395B47 %
70°C,22hr3ASTM D395B27 %
70°C,22hr2ASTM D395B31 %
Shore hardness--2ASTM D263252 %
--3ASTM D263252 %
tear strength--4,3ASTM D62483.0 kN/m
--4,2ASTM D62470.1 kN/m
Split3ASTM D47020 kN/m
Split2ASTM D47019 kN/m
tensile strength--2ASTM D41239.2 MPa
300%Strain3ASTM D4128.54 MPa
300%Strain2ASTM D4128.06 MPa
100%Strain3ASTM D4126.29 MPa
100%Strain2ASTM D4126.17 MPa
--3ASTM D41242.2 MPa