Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
EVA V26061 ASIA POLYMER TAIWAN
POLYMER-E 
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Basic performanceTest ConditionTest MethodASIA POLYMER TAIWAN/V26061
densityASTM D-15050.951 g/cm³
Vinyl acetate contentAPC Method26 %
melt mass-flow rateASTM D-12385.5 g/10min
Mechanical propertiesTest ConditionTest MethodASIA POLYMER TAIWAN/V26061
elongation薄膜ASTM D-638780 %
tensile strength 薄膜,断裂ASTM D-638200 kg/cm2
Shore hardnessShore DASTM D-224030
Thermal performanceTest ConditionTest MethodASIA POLYMER TAIWAN/V26061
Low temperature brittleness temperatureASTM D-746<-70 °C
vicatASTM D-152550 °C
melting temperatureAPC Method71 °C