plas
Log In

Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PP Homopolymer TOLEN H040 GP SIBUR RUSSIA
--
currency
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

thermal performanceTest ConditionTest MethodSIBUR RUSSIA/TOLEN H040 GP
Hot deformation temperature0.45MPa,UnannealedInternal Method80.0 °C
Vicat softening temperatureInternal Method4156 °C
mechanical propertiesTest ConditionTest MethodSIBUR RUSSIA/TOLEN H040 GP
Bending modulusInternal Method1500 MPa
Tensile strainYieldInternal Method11 %
tensile strengthYieldInternal Method30.0 MPa
Physical propertiesTest ConditionTest MethodSIBUR RUSSIA/TOLEN H040 GP
melt mass-flow rate230°C/2.16kgInternal Method4.0 g/10min
impact performanceTest ConditionTest MethodSIBUR RUSSIA/TOLEN H040 GP
Impact strength of cantilever beam gap23°CInternal Method2.0 kJ/m²