Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

EVA LD 728.61 EXXONMOBIL USA
Escorene™
Profile
high strength,Bi-Sn ,High toughness
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| hardness | Test Condition | Test Method | EXXONMOBIL USA/LD 728.61 |
|---|---|---|---|
| Shore hardness | ShoreD,15Sec | ASTM D2240 | 36 |
| ShoreA,15Sec | ASTM D2240 | 76 |
| thermal performance | Test Condition | Test Method | EXXONMOBIL USA/LD 728.61 |
|---|---|---|---|
| Vicat softening temperature | ASTM D1525 | 64.0 °C |
| mechanical properties | Test Condition | Test Method | EXXONMOBIL USA/LD 728.61 |
|---|---|---|---|
| Bending modulus | 1%Secant | ASTM D790 | 60.3 Mpa |
| elongation | Yield | ASTM D638 | 260 % |
| Break | ASTM D638 | >800 % | |
| tensile strength | Yield | ASTM D638 | 5.24 Mpa |
| Break | ASTM D638 | 11.4 Mpa |
| Physical properties | Test Condition | Test Method | EXXONMOBIL USA/LD 728.61 |
|---|---|---|---|
| melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 2.0 g/10min |
| Vinyl acetate content | ASTM D-256-97 | 18.2 wt% |
| impact performance | Test Condition | Test Method | EXXONMOBIL USA/LD 728.61 |
|---|---|---|---|
| Dart impact | 23°C | ASTM D3763 | 17.6 J |
| -40°C | ASTM D3763 | 35.3 J |