plas
Log In

Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
TPU 3690AU Taiwan Bayer Youde
Desmopan® 
pipeline,film,Footwear
wear resistant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

hardnessTest ConditionTest MethodTaiwan Bayer Youde/3690AU
Shore hardnessShore D, 15 secISO 868240
Shore D, 1 Sec, 23°CISO 761940
Shore A, 1 Sec, 23°CISO 761991
Shore A, 3 secISO 868291
mechanical propertiesTest ConditionTest MethodTaiwan Bayer Youde/3690AU
Tensile storage modulus20°CISO 672194.0 Mpa
-20°CISO 6721940 Mpa
60°CISO 672154.0 Mpa
Tensile strainBreak, 23°CDIN 53504510 %
tensile strengthBreak, 23°CDIN 5350460.2 Mpa
100% Strain, 23°CDIN 5350410.0 Mpa
300% Strain, 23°CDIN 5350423.9 Mpa
10% Strain, 23°CDIN 535043.50 Mpa
50% Strain, 23°CDIN 535048.00 Mpa
Wear resistanceISO 464925.0 mm³
squeeze outTest ConditionTest MethodTaiwan Bayer Youde/3690AU
drying temperature< 80 °C
Melt Temperature180 to 200 °C
elastomerTest ConditionTest MethodTaiwan Bayer Youde/3690AU
Permanent compression deformation70°C, 24 hr6ISO 81525 %
23°C, 72 hrISO 81521 %
70°C, 24 hr4ISO 81542 %
ResilienceISO 466229 %
tear strength23°CISO 34-195 kN/m
injectionTest ConditionTest MethodTaiwan Bayer Youde/3690AU
drying temperature< 80 °C
Mold temperature20 to 40 °C
Processing (melt) temperature215 to 235 °C