plas

Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PC/ABS FR3000 700584 COVESTRO GERMANY
Bayblend® 
Electrical field,Electronic field,Household appliances,Household appliances,Automotive sector
Flame retardant,UV resistance,High mobility
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

thermal performanceTest ConditionTest MethodCOVESTRO GERMANY/FR3000 700584
Hot deformation temperature0.45 MPa, UnannealedISO 75-2/B95.0 °C
1.8 MPa, UnannealedISO 75-2/A85.0 °C
Vicat softening temperatureISO 306/B120103 °C
mechanical propertiesTest ConditionTest MethodCOVESTRO GERMANY/FR3000 700584
Nominal tensile fracture strain23°CISO 527-2/5040 %
Tensile modulus23°CISO 527-2/12650 Mpa
Tensile strainYield, 23°CISO 527-2/503.9 %
tensile strengthYield, 23°CISO 527-2/5064.0 Mpa
Electrical performanceTest ConditionTest MethodCOVESTRO GERMANY/FR3000 700584
Relative permittivity23°C, 100 HzIEC 602503.00
23°C, 1 MHzIEC 602502.90
Surface resistivityIEC 600931.0E+16 ohms
Volume resistivity23°CIEC 600931.0E+16 ohms·cm
Physical propertiesTest ConditionTest MethodCOVESTRO GERMANY/FR3000 700584
density23°CISO 11831.18 g/cm³
Melt Volume Flow Rate (MVR)240°C/5.0 kgISO 113320.0 cm3/10min
Shrinkage rate横向FlowISO 25770.40 - 0.60 %
FlowISO 25770.40 - 0.60 %
Water absorption rateSaturation, 23°CISO 620.40 %
Equilibrium, 23°C, 50% RHISO 620.10 %
impact performanceTest ConditionTest MethodCOVESTRO GERMANY/FR3000 700584
Impact strength of cantilever beam gap23°CISO 180/A30 kJ/m²
flammabilityTest ConditionTest MethodCOVESTRO GERMANY/FR3000 700584
Extreme Oxygen IndexISO 4589-234 %
UL flame retardant rating2.0 mmUL 945VB
1.5 mmUL 94V-0
Filling analysisTest ConditionTest MethodCOVESTRO GERMANY/FR3000 700584
ISOPC+ABS-FR(40)
Melt viscosity240°CISO 11443-A150 Pa·s
injectionTest ConditionTest MethodCOVESTRO GERMANY/FR3000 700584
Back pressure5.00 to 15.0 Mpa
Drying Temperature - Dry Air Dryer80 °C
Drying time - Dry Air Dryer4.0 hr
Exhaust hole depth0.025 to 0.075 mm
Mold temperature60 to 90 °C
Processing (melt) temperature240 to 270 °C
Spray nozzle temperature255 to 265 °C
Suggested injection volume30 to 70 %
Suggested maximum moisture content< 0.020 %
Temperature at the front of the material cylinder230 to 240 °C
Temperature at the rear of the barrel220 to 230 °C
Temperature in the middle of the barrel225 to 235 °C