| thermal performance | Test Condition | Test Method | BOREALIS EUROPE/ED213AE |
|---|---|---|---|
| Vicat softening temperature | -- | ISO 306/B50 | 40.0 °C |
| Linear coefficient of thermal expansion | MD:-30to80°C | Internal Method | 7E-05 cm/cm/°C |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 102 °C |
| MeltEnergy | ISO 11357 | 56.4 kJ/kg | |
| Vicat softening temperature | -- | ISO 306/A50 | 124 °C |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 54.0 °C |
| impact performance | Test Condition | Test Method | BOREALIS EUROPE/ED213AE |
| Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 29 kJ/m² |
| -30°C | ISO 179/1eA | 4.5 kJ/m² | |
| -20°C | ISO 179/1eA | 10 kJ/m² | |
| Impact strength of cantilever beam gap | 23°C | ISO 180/1A | 25 kJ/m² |
| -20°C | ISO 180/1A | 8.0 kJ/m² | |
| Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 110 kJ/m² |
| -20°C | ISO 179/1eU | 44 kJ/m² | |
| Physical properties | Test Condition | Test Method | BOREALIS EUROPE/ED213AE |
| density | ISO 1183 | 1.02 g/cm³ | |
| Shrinkage rate | Internal Method | 0.60 % | |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 8.0 g/10min |
| mechanical properties | Test Condition | Test Method | BOREALIS EUROPE/ED213AE |
| tensile strength | Yield,Injection | ISO 527-2/50 | 17.0 Mpa |
| Tensile modulus | Injection | ISO 527-2/1 | 1750 Mpa |
| Bending modulus | Injection | ISO 178 | 1850 Mpa |
| bending strength | Injection | ISO 178 | 24.0 Mpa |
| Tensile strain | Yield,Injection | ISO 527-2/50 | 4.0 % |
| hardness | Test Condition | Test Method | BOREALIS EUROPE/ED213AE |
| Ball Pressure Test | H132/10 | ISO 2039-1 | 40.0 Mpa |