Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PUR 7501 DPLF/442 USA Anderson
--
--
liquid
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Other performance | Test Condition | Test Method | USA Anderson/7501 DPLF/442 |
|---|---|---|---|
| storage stability | 2.0 to 3.0 min |
| Test Condition | Test Method | USA Anderson/7501 DPLF/442 | |
|---|---|---|---|
| elongation | Break | ASTM D412 | 180 % |
| Post curing time | 100°C | 16 hr | |
| Shore hardness | Shore D | ASTM D2240 | 76 |
| Shrinkage rate | Flow | ASTM D955 | 1.3 % |
| stripping time | 100°C | 10 min | |
| tensile strength | Yield | ASTM D412 | 44.8 MPa |
| mechanical properties | Test Condition | Test Method | USA Anderson/7501 DPLF/442 |
|---|---|---|---|
| tensile strength | 100%Strain | ASTM D412 | 37.9 MPa |
| Physical properties | Test Condition | Test Method | USA Anderson/7501 DPLF/442 |
|---|---|---|---|
| density | ASTM D1505 | 1.22 g/cm³ |