| Electrical performance | Test Condition | Test Method | TORAY JAPAN/A900 |
|---|---|---|---|
| Dissipation factor | 23°C,1MHz | IEC 60250 | 1E-03 |
| Volume resistivity | IEC 60093 | 1E+16 ohms·cm | |
| Dielectric constant | 23°C,1MHz | IEC 60250 | 3.50 |
| Dielectric strength | IEC 60243-1 | 30 KV/mm | |
| mechanical properties | Test Condition | Test Method | TORAY JAPAN/A900 |
| tensile strength | Yield,23°C | ISO 527-2 | 85.0 Mpa |
| Bending modulus | 23°C | ISO 178 | 3900 Mpa |
| bending strength | 23°C | ISO 178 | 140 Mpa |
| Tensile strain | Break,23°C | ISO 527-2 | 8.0 % |
| Physical properties | Test Condition | Test Method | TORAY JAPAN/A900 |
| Water absorption rate | 23°C,24hr | ISO 62 | 0.020 % |
| Shrinkage rate | TD:3.00mm2 | Internal Method | 1.9 % |
| MD:3.00mm4 | Internal Method | 1.4 % | |
| flammability | Test Condition | Test Method | TORAY JAPAN/A900 |
| UL flame retardant rating | UL 94 | V-0 | |
| impact performance | Test Condition | Test Method | TORAY JAPAN/A900 |
| Impact strength of simply supported beam without notch | 23°C | ISO 179 | 50 kJ/m² |
| thermal performance | Test Condition | Test Method | TORAY JAPAN/A900 |
| Linear coefficient of thermal expansion | TD | ISO 11359-2 | 6.6E-05 cm/cm/°C |
| MD | ISO 11359-2 | 6.2E-05 cm/cm/°C | |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 105 °C |
| Melting temperature | ISO 11357-3 | 278 °C | |
| Supplementary Information | Test Condition | Test Method | TORAY JAPAN/A900 |
| BarFlowLength | 320°C,1.00mm | Internal Method | 200 mm |