Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

HDPE J4406-6(QHJ02) SINOPEC QILU
--
Local cable insulation la
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Other performance | Test Condition | Test Method | SINOPEC QILU/J4406-6(QHJ02) |
---|---|---|---|
hydrolysis resistance | GB 1409 | 合格 | |
Color | YD/T760-95 | 本色 | |
Oxidation induction period (Cu cup) | GB 2951.37 | 146 min |
Basic performance | Test Condition | Test Method | SINOPEC QILU/J4406-6(QHJ02) |
---|---|---|---|
density | GB 1033 | 0.942 g/cm³ | |
melt mass-flow rate | GB 3682 | 0.8 g/10min |
Mechanical properties | Test Condition | Test Method | SINOPEC QILU/J4406-6(QHJ02) |
---|---|---|---|
elongation | 断裂 | GB 1040 | 640 % |
Environmental stress cracking resistance | 48h | YD/T760-95 | 0/10 失效数 |
tensile strength | GB 1040 | 20.3 Mpa |
Electrical performance | Test Condition | Test Method | SINOPEC QILU/J4406-6(QHJ02) |
---|---|---|---|
dielectric constant | 1MHZ | GB 1409 | 2.3 |
Dielectric loss | 1MHZ | GB 1409 | 1.54×10-4 |
Volume resistivity | GB 1410 | 3.16×1014 Ω·M |
Thermal performance | Test Condition | Test Method | SINOPEC QILU/J4406-6(QHJ02) |
---|---|---|---|
Environmental Stress Cracking Resistance (ESCR) | 96h | YD/T760-95 | 0/9 失效数 |
Low temperature brittleness temperature | -76℃ | GB 5470 | 0/10 失效数 |