Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 K224-PG3 DSM HOLAND
Akulon®
--
Impact modification
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Mechanical properties | Test Condition | Test Method | DSM HOLAND/K224-PG3 |
---|---|---|---|
Charpy Notched Impact Strength | 23℃ | ISO 179/1eA | 2.5 J/cm |
Tensile modulus | ISO 527-1/-2 | 2.6 Gpa | |
Charpy Notched Impact Strength | -30℃ | ISO 179/1eA | 0.8 J/cm |
elongation at break | ASTM D638/ISO 527 | 7 % | |
Impact strength of simply supported beam without notch | -30℃ | ISO 179/1eU | 7.5 J/cm |
Electrical performance | Test Condition | Test Method | DSM HOLAND/K224-PG3 |
---|---|---|---|
Compared to the Leakage Traceability Index (CTI) | IEC 60112 | 500 V | |
dielectric strength | IEC 60243-1 | kV/mm | |
Dielectric loss | 1E+6HZ | IEC 60250 | 0.12 |
dielectric constant | IEC 60250 | ||
Volume resistivity | IEC 60093 | ≥1.0E+15 Ohm.cm | |
Surface Resistivity | IEC 60093 | ≥1.0E+15 Ohm | |
Dielectric loss | 100Hz | IEC 60250 | 0.15 |
Physical properties | Test Condition | Test Method | DSM HOLAND/K224-PG3 |
---|---|---|---|
density | ASTM D792/ISO 1183 | 1.2 |
physical property | Test Condition | Test Method | DSM HOLAND/K224-PG3 |
---|---|---|---|
Water absorption rate | ISO 62 | 6.8 % | |
Hygroscopic balance | ISO 62 | 2 % |
Contact Us
Get App
Top