| hardness | Test Condition | Test Method | SK KOREA/8605L |
|---|---|---|---|
| Shore hardness | Shore A, 1 Sec, Compression Molded | ASTM D2240 | 66 |
| Shore D, 1 Sec, Compression Molded | ASTM D2240 | 17 | |
| mechanical properties | Test Condition | Test Method | SK KOREA/8605L |
| Tensile modulus | Compression Molded,100% Secant | ASTM D638 | 1.86 Mpa |
| Bending modulus | Compression Molded,% Secant | ASTM D790 | 8.34 Mpa |
| tensile strength | Break, Compression Molded | ASTM D638 | 6.08 Mpa |
| elongation | Break, Compression Molded | ASTM D638 | > 1000 % |
| Physical properties | Test Condition | Test Method | SK KOREA/8605L |
| Mooney viscosity | ML 1+4, 121°C | ASTM D1646 | 36 MU |
| melt mass-flow rate | 190°C/2.16 kg | ASTM D1238 | 0.50 g/10 min |
| thermal performance | Test Condition | Test Method | SK KOREA/8605L |
| Glass transition temperature | Internal Method | -56.0 °C | |
| Melting temperature | Internal Method | 45.0 °C | |
| elastomer | Test Condition | Test Method | SK KOREA/8605L |
| tear strength | ASTM D624 | 33.3 kN/m |