EPDM Precision Polymer E60H Precision Polymer Engineering Ltd.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Supplementary Information | Test Condition | Test Method | Precision Polymer Engineering Ltd./Precision Polymer E60H |
---|---|---|---|
Low temperature resistance | -老化后非脆性 | ISO R812 | -45 °C |
-老化后非脆性 | ASTM D2137 | -45 °C |
hardness | Test Condition | Test Method | Precision Polymer Engineering Ltd./Precision Polymer E60H |
---|---|---|---|
IRHD hardness | ASTMD1415 | 60 |
elastomer | Test Condition | Test Method | Precision Polymer Engineering Ltd./Precision Polymer E60H |
---|---|---|---|
elongation | 断裂 | ASTMD412 | 250 % |
compression set | 100°C,24hr | ASTM D395B | 64 % |
tensile strength | 屈服 | ASTMD412 | 13.8 MPa |
compression set | 100°C,24hr2 | ISO 815 | 64 % |
aging | Test Condition | Test Method | Precision Polymer Engineering Ltd./Precision Polymer E60H |
---|---|---|---|
Change rate of tensile strength in air | 125°C,168hr | ASTMD412 | -20 % |
Change rate of ultimate elongation in air | 125°C,168hr | ASTMD412 | -20 % |
Change rate of IRHD hardness in the air | 125°C,168hr | ASTMD573 | 15 |
Thermal performance | Test Condition | Test Method | Precision Polymer Engineering Ltd./Precision Polymer E60H |
---|---|---|---|
maximum service temperature | 150 °C |