Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

POM K100HS KOLON KOREA
KOCETAL®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | KOLON KOREA/K100HS |
---|---|---|---|
Rockwell hardness | M级 | ASTMD785 | 78 |
Electrical performance | Test Condition | Test Method | KOLON KOREA/K100HS |
---|---|---|---|
Volume resistivity | ASTMD257 | 1E+14 ohms·cm | |
Dissipation Factor | 1MHz | ASTMD150 | 6E-03 |
dielectric constant | ASTMD150 | 3.70 | |
dielectric strength | ASTMD149 | 19 KV/mm | |
Surface Resistivity | ASTMD257 | 1E+16 ohms |
Mechanical properties | Test Condition | Test Method | KOLON KOREA/K100HS |
---|---|---|---|
Flexural modulus | 23°C | ASTMD790 | 2200 Mpa |
elongation | 屈服,23°C | ASTMD638 | 80 % |
tensile strength | 屈服,23°C | ASTMD638 | 57.0 Mpa |
bending strength | 23°C | ASTMD790 | 80.0 Mpa |
flammability | Test Condition | Test Method | KOLON KOREA/K100HS |
---|---|---|---|
UL flame retardant rating | UL94 | HB |
physical property | Test Condition | Test Method | KOLON KOREA/K100HS |
---|---|---|---|
melt mass-flow rate | 190°C/2.16kg | ASTMD1238 | 2.5 g/10min |
Shrinkage rate | MD | ASTMD955 | 2.2 % |
Water absorption rate | 平衡,23°C,60%RH | ASTMD570 | 0.22 % |
Thermal performance | Test Condition | Test Method | KOLON KOREA/K100HS |
---|---|---|---|
MD | ASTMD696 | 1.3E-04 cm/cm/°C | |
0.45MPa,未退火 | ASTMD648 | 158 °C | |
melting temperature | 166 °C | ||
vicat | ASTMD1525 | 162 °C | |
1.8MPa,未退火 | ASTMD648 | 110 °C |