PC+AS TARFLON™ SK3731 IDEMITSU JAPAN
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | IDEMITSU JAPAN/TARFLON™ SK3731 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179 | 4.0 kJ/m² |
Supplementary Information | Test Condition | Test Method | IDEMITSU JAPAN/TARFLON™ SK3731 |
---|---|---|---|
ISO Shortcut | >PC+AS-(TD+PD)30-FR(40)< |
Mechanical properties | Test Condition | Test Method | IDEMITSU JAPAN/TARFLON™ SK3731 |
---|---|---|---|
Nominal tensile fracture strain | ISO 527-2 | 2.0 % | |
tensile strength | 屈服 | ISO 527-2 | 74.0 MPa |
Flexural modulus | ISO 178 | 7500 MPa | |
bending strength | ISO 178 | 106 MPa |
flammability | Test Condition | Test Method | IDEMITSU JAPAN/TARFLON™ SK3731 |
---|---|---|---|
UL flame retardant rating | 2.0mm | UL 94 | 5VB |
1.5mm | UL 94 | V-1 |
physical property | Test Condition | Test Method | IDEMITSU JAPAN/TARFLON™ SK3731 |
---|---|---|---|
spiral flow length | 内部方法 | 21.0 cm | |
Shrinkage rate | TD:2.00mm | 内部方法 | 0.20 % |
Melt volume flow rate | 260°C/2.16kg | ISO 1133 | 8.00 cm³/10min |
Shrinkage rate | MD:2.00mm | 内部方法 | 0.17 % |
density | ISO 1183 | 1.43 g/cm³ |
Thermal performance | Test Condition | Test Method | IDEMITSU JAPAN/TARFLON™ SK3731 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 105 °C |
Linear coefficient of thermal expansion | MD | ISO 11359-2 | 2.7E-05 cm/cm/°C |
RTI Imp | UL 746 | 50.0 °C | |
Linear coefficient of thermal expansion | TD | ISO 11359-2 | 4.4E-05 cm/cm/°C |
RTI Str | UL 746 | 50.0 °C | |
RTI Elec | UL 746 | 50.0 °C |