Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

ASA/PC 2864 BK BASF GERMANY
Luran®S
Application in the automotive field
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | BASF GERMANY/2864 BK |
---|---|---|---|
Ball Pressure Test | ISO 2039-1 | 110 Mpa |
film | Test Condition | Test Method | BASF GERMANY/2864 BK |
---|---|---|---|
elongation | Break | ISO 527-3 | >50 % |
thermal performance | Test Condition | Test Method | BASF GERMANY/2864 BK |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Annealed | ISO 75-2/A | 105 °C |
0.45MPa,Annealed | ISO 75-2/B | 124 °C | |
Linear coefficient of thermal expansion | MD | ISO 11359-2 | 7.0E-5到9.0E-5 cm/cm/°C |
thermal conductivity | DIN 52612 | 0.17 W/m/K | |
Vicat softening temperature | -- | ISO 306/B50 | 120 °C |
-- | ISO 306/A50 | 134 °C |
mechanical properties | Test Condition | Test Method | BASF GERMANY/2864 BK |
---|---|---|---|
bending strength | ISO 178 | 100 Mpa | |
Tensile modulus | ISO 527-2 | 2600 Mpa | |
Tensile strain | Yield,23°C | ISO 527-2 | 4.6 % |
tensile strength | Yield,23°C | ISO 527-2 | 63.0 Mpa |
Electrical performance | Test Condition | Test Method | BASF GERMANY/2864 BK |
---|---|---|---|
Dielectric constant | 100Hz | IEC 60250 | 3.10 |
Dissipation factor | 1MHz | IEC 60250 | 0.012 |
100Hz | IEC 60250 | 6E-03 | |
Surface resistivity | IEC 60093 | 1E+13 ohms | |
Volume resistivity | IEC 60093 | 1E+14 ohms·cm |
Physical properties | Test Condition | Test Method | BASF GERMANY/2864 BK |
---|---|---|---|
Melt Volume Flow Rate (MVR) | 220°C/10.0kg | ISO 1133 | 10.0 cm3/10min |
260°C/5.0kg | ISO 1133 | 25.0 cm3/10min | |
Shrinkage rate | ISO 294-4 | 0.50-0.90 % | |
Water absorption rate | Equilibrium,23°C,50%RH | ISO 62 | 0.18 % |
Saturation,23°C | ISO 62 | 0.60 % |