plas
Log In

Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PA6 Polimid B 40 Poliblend S.p.a.
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

thermal performanceTest ConditionTest MethodPoliblend S.p.a./Polimid B 40
Ball Pressure Test165°CIEC 60695-10-2通过
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B180 °C
1.8MPa,UnannealedISO 75-2/A80.0 °C
连续使用温度280.0 °C
Melting temperatureDSC222 °C
Vicat softening temperatureISO 306/A120208 °C
mechanical propertiesTest ConditionTest MethodPoliblend S.p.a./Polimid B 40
Tensile modulusISO 527-22900 MPa
Tensile strainYieldISO 527-25.5 %
BreakISO 527-2>100 %
tensile strengthYieldISO 527-285.0 MPa
Electrical performanceTest ConditionTest MethodPoliblend S.p.a./Polimid B 40
Compared to the anti leakage trace indexIEC 60112PLC 0
Physical propertiesTest ConditionTest MethodPoliblend S.p.a./Polimid B 40
densityISO 11831.14 g/cm³
Shrinkage rate1.0to1.4 %
Water absorption rate23°C,24hrISO 622.0 %
impact performanceTest ConditionTest MethodPoliblend S.p.a./Polimid B 40
Impact strength of cantilever beam gapISO 180/A6.5 kJ/m²
Suspended wall beam without notch impact strengthISO 180无断裂
flammabilityTest ConditionTest MethodPoliblend S.p.a./Polimid B 40
Burning wire flammability index2.0mmIEC 60695-2-12825 °C
UL flame retardant rating3.2mmUL 94V-2
0.8mmUL 94V-2
1.6mmUL 94V-2