Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC/ABS 7570 BK STYRON US
EMERGE™
Tool handle,TV casing,Electrical enclosure,Electrical/Electronic Applications,Shell,LCD,application
Flame retardant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | STYRON US/7570 BK |
---|---|---|---|
Ball pressure temperature | IEC 60335-1 | 95.0 °C | |
Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 90.0 °C |
1.8MPa,Unannealed | ISO 75-2/A | 80.0 °C | |
Vicat softening temperature | -- | ISO 306/A120 | 105 °C |
-- | ISO 306/B50 | 98.0 °C |
mechanical properties | Test Condition | Test Method | STYRON US/7570 BK |
---|---|---|---|
Bending modulus | 4.00mm,InjectionMolded | ISO 178 | 2700 Mpa |
bending strength | 4.00mm,InjectionMolded | ISO 178 | 92.0 Mpa |
Tensile modulus | 4.00mm,Injection | ISO 527-2/1 | 2600 Mpa |
Tensile strain | Break,4.00mm,Injection | ISO 527-2/50 | 40 % |
Yield,4.00mm,InjectionMolded | ISO 527-2/50 | 4.0 % | |
tensile strength | Break,4.00mm,Injection | ISO 527-2/50 | 47.0 Mpa |
Yield,4.00mm,InjectionMolded | ISO 527-2/50 | 60.0 Mpa |
Physical properties | Test Condition | Test Method | STYRON US/7570 BK |
---|---|---|---|
Apparent density | ISO 60 | 0.67 g/cm³ | |
melt mass-flow rate | 230°C/3.8kg | ISO 1133 | 20 g/10min |
260°C/5.0kg | ISO 1133 | 95 g/10min | |
Shrinkage rate | MD | ISO 294-4 | 0.40-0.60 % |
flammability | Test Condition | Test Method | STYRON US/7570 BK |
---|---|---|---|
Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 960 °C |
Ignition temperature of heating wire | 2.0mm | IEC 60695-2-13 | 800 °C |
UL flame retardant rating | 2.5mm | UL 94 | V-0 |
1.6mm | UL 94 | V-0 |