PA66 A3ZG6 BASF GERMANY
Ultramid®
Shell
Oil resistant,Impact modification,Low temperature impact re
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Mechanical properties | Test Condition | Test Method | BASF GERMANY/A3ZG6 |
---|---|---|---|
Tensile modulus | ASTM D638/ISO 527 | 8500/6000 kg/cm²(MPa)[Lb/in²] | |
Charpy Notched Impact Strength | ASTM D256/ISO 179 | 10/_ kg·cm/cm(J/M)ft·lb/in | |
Flexural modulus | ASTM D790/ISO 178 | 7300/4900 kg·cm/cm(J/M)ft·lb/in | |
bending strength | ASTM D790/ISO 178 | 210/150 kg·cm/cm(J/M)ft·lb/in |
Physical properties | Test Condition | Test Method | BASF GERMANY/A3ZG6 |
---|---|---|---|
density | ASTM D792/ISO 1183 | 1.33 | |
Water absorption rate | ASTM D570/ISO 62 | 4.7-5.3 % |
Thermal performance | Test Condition | Test Method | BASF GERMANY/A3ZG6 |
---|---|---|---|
Combustibility (rate) | UL 94 | HB | |
melting temperature | 280~300 ℃(℉) |