Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA6 Razamid® B111 GR35 Razin? Engineering Plastics
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | Razin? Engineering Plastics/Razamid® B111 GR35 |
---|---|---|---|
Impact strength of cantilever beam gap | 23°C | ASTM D256 | 18.0 kJ/m² |
Electrical performance | Test Condition | Test Method | Razin? Engineering Plastics/Razamid® B111 GR35 |
---|---|---|---|
dielectric strength | ASTM D149 | 18 kV/mm | |
Volume resistivity | IEC 60093 | 1E+13 ohms·cm | |
Surface Resistivity | IEC 60093 | 1E+12 ohms | |
dielectric constant | ASTM D150 | 3.80 |
Mechanical properties | Test Condition | Test Method | Razin? Engineering Plastics/Razamid® B111 GR35 |
---|---|---|---|
elongation | 断裂 | ASTM D638 | 3.0 % |
Flexural modulus | ASTM D790 | 10500 MPa | |
tensile strength | 屈服 | ASTM D638 | 195 MPa |
bending strength | ASTM D790 | 280 MPa |
physical property | Test Condition | Test Method | Razin? Engineering Plastics/Razamid® B111 GR35 |
---|---|---|---|
Shrinkage rate | MD | ASTM D955 | 0.70 % |
density | ASTM D792 | 1.41 g/cm³ |
Thermal performance | Test Condition | Test Method | Razin? Engineering Plastics/Razamid® B111 GR35 |
---|---|---|---|
Heat distortion temperature | 1.8MPa,未退火,HDT | ASTM D648 | 212 °C |
vicat | ASTM D1525 | 210 °C | |
Heat distortion temperature | 0.45MPa,未退火,HDT | ASTM D648 | 220 °C |
melting temperature | ASTM D3418 | 225 °C |