Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PA66 ECO366H NT0708 ASCEND USA
Vydyne®
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Electrical performance | Test Condition | Test Method | ASCEND USA/ECO366H NT0708 |
---|---|---|---|
Dissipation Factor | 耐电弧性 | IEC61621 | 120-179 S |
Dielectric Strength | 1.0mm | IEC60243-1 | 17 KV/mm |
IEC60093 | 1E+10 Ω.cm | ||
Dissipation Factor | 相对漏电起痕指数 | IEC60112 | 600 V |
Mechanical properties | Test Condition | Test Method | ASCEND USA/ECO366H NT0708 |
---|---|---|---|
Charpy Notched Impact Strength | -30°C | ISO179/1eA | 3.4 kJ/m² |
Impact strength of simply supported beam without notch | 23°C | ISO179/1eU | 78 kJ/m² |
-30°C | ISO179/1eU | 75 kJ/m² | |
Flexural modulus | 23°C | ISO178 | 3900 Mpa |
Impact strength of cantilever beam gap | 23°C | ISO180/1A | 6.0 kJ/m² |
elongation at break | 23°C | ISO527-2 | 4.0 % |
Charpy Notched Impact Strength | 23°C | ISO179/1eA | 3.7 kJ/m² |
bending strength | 23°C | ISO178 | 104 Mpa |
Tensile modulus | 泊松比 | ISO527-2 | 0.40 |
tensile strength | 屈服,23°C | ISO527-2 | 83 Mpa |
Flame retardant performance | Test Condition | Test Method | ASCEND USA/ECO366H NT0708 |
---|---|---|---|
fire rating | 氧指数 | ISO4589-2 | 24 % |
UL-94 | 3.00mm V-0 |
physical property | Test Condition | Test Method | ASCEND USA/ECO366H NT0708 |
---|---|---|---|
Water absorption rate | (23°C,50RH) | ISO62 | 2.3 % |
Shrinkage rate | MD2.0mm | ISO294-4 | 0.90 % |
Water absorption rate | (23°C,24hr) | ISO62 | 0.80 % |
Shrinkage rate | TD2.0mm | ISO294-4 | 0.60 % |
Thermal performance | Test Condition | Test Method | ASCEND USA/ECO366H NT0708 |
---|---|---|---|
Heat distortion temperature | 1.80MPa退火 | ISO75-2/Af | 75 °C |
熔点 | ISO11359-2 | 265 °C | |
0.45MPa未退火 | ISO75-2/Bf | 240 °C |