Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC NH-3200 FW9661 Samsung Cheil South Korea
INFINO®
Audio and video equipment,Laptop,Electronic and Electrical Applications
Glass fiber reinforced,Flame retardant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | Samsung Cheil South Korea/NH-3200 FW9661 |
---|---|---|---|
Rockwell hardness | R -Sale | ISO 2039-2 | 120 |
R-Scale | ASTM D785 | 120 |
thermal performance | Test Condition | Test Method | Samsung Cheil South Korea/NH-3200 FW9661 |
---|---|---|---|
Hot deformation temperature | 0.45 MPa, Unannealed, 4.00 mm | ISO 75-2/B | 102 °C |
1.8 MPa, Unannealed, 4.00 mm | ISO 75-2/A | 97.0 °C | |
0.45 MPa, Unannealed, 6.40 mm | ASTM D648 | 105 °C | |
1.8 MPa, Unannealed, 6.40 mm | ASTM D648 | 100 °C |
mechanical properties | Test Condition | Test Method | Samsung Cheil South Korea/NH-3200 FW9661 |
---|---|---|---|
Bending modulus | --5 | ISO 178 | 6000 Mpa |
--4 | ASTM D790 | 5900 Mpa | |
bending strength | --5 | ISO 178 | 150 Mpa |
--4 | ASTM D790 | 150 Mpa | |
elongation | Break | ISO 527-2/5 | 3.0 % |
Break3 | ASTM D638 | 3.0 % | |
Tensile modulus | -- | ISO 527-2/5 | 5000 Mpa |
--3 | ASTM D638 | 4900 Mpa | |
tensile strength | Break | ISO 527-2/5 | 120 Mpa |
Yield | ISO 527-2/5 | 120 Mpa | |
Break3 | ASTM D638 | 120 Mpa | |
Yield3 | ASTM D638 | 120 Mpa |
Physical properties | Test Condition | Test Method | Samsung Cheil South Korea/NH-3200 FW9661 |
---|---|---|---|
melt mass-flow rate | 250°C/5.0 kg | ASTM D1238 | 19 g/10 min |
300°C/1.2 kg | ASTM D1238 | 12 g/10 min | |
Shrinkage rate | 横向Flow : 2.00 mm | ISO 294-4 | 0.10 - 0.40 % |
Across FlowFlow : 3.20 mm | ASTM D955 | 0.10 - 0.40 % | |
Flow : 3.20 mm | ASTM D955 | 0.10 - 0.40 % | |
Flow : 2.00 mm | ISO 294-4 | 0.10 - 0.40 % |
flammability | Test Condition | Test Method | Samsung Cheil South Korea/NH-3200 FW9661 |
---|---|---|---|
UL flame retardant rating | 3.0 mm | UL 94 | V-0 |
0.75 mm | UL 94 | V-0 | |
0.830mm | UL 94 | V-0 |
injection | Test Condition | Test Method | Samsung Cheil South Korea/NH-3200 FW9661 |
---|---|---|---|
Back pressure | 0.981 to 1.96 Mpa | ||
Hot air dryer | 3.0 to 4.0 hr | ||
80 °C | |||
Injection pressure | 98.1 Mpa | ||
Mold temperature | 60 to 70 °C | ||
Screw speed | 30 to 100 rpm | ||
Spray nozzle temperature | 270 °C | ||
Suggested maximum moisture content | 0.040 % | ||
Temperature at the front of the material cylinder | 260 to 280 °C | ||
Temperature at the rear of the barrel | 260 to 270 °C | ||
Temperature in the middle of the barrel | 270 to 290 °C | ||
Vacuum drying machine | 4.0 to 6.0 hr | ||
80 °C |