Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
POM 311DP DUPONT USA
Delrin®
Fitness equipment、Automotive components
High temperature resistan、wear resistant
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Thermal PropertiesTest ConditionTest MethodDUPONT USA/311DP
Annealing Time-Optional30.0 min/mm
Heat Deflection Temperature1.8MPa,未退火ISO75-2/A103 °C
Melting TemperatureISO11357-3178 °C
Annealing Temperature160 °C
AdditionalTest ConditionTest MethodDUPONT USA/311DP
EmissionofOrganicCompoundsVDA2777.30 µgC/g
EmissionVDA275<8.00 mg/kg
PhysicalTest ConditionTest MethodDUPONT USA/311DP
Density / Specific GravityISO11831.42 g/cm³
Melt Mass-Flow Rate190°C/2.16kgISO11337.0 g/10min
Mechanical PropertiesTest ConditionTest MethodDUPONT USA/311DP
Tensile Strain屈服ISO527-215 %
Tensile Stress屈服ISO527-275.0 Mpa
Nominal Tensile Strain at BreakISO527-228 %
Tensile ModulusISO527-23300 Mpa
Impact PropertiesTest ConditionTest MethodDUPONT USA/311DP
Charpy Notched Impact Strength-30°CISO179/1eA8.0 kJ/m²
23°CISO179/1eA9.0 kJ/m²
FlammabilityTest ConditionTest MethodDUPONT USA/311DP
Burning Rate1.00mmISO3795<100 mm/min
Flame Rating1.5mmIEC60695-11-10,-20HB
0.8mmIEC60695-11-10,-20HB
Fogging-G-valuecondensateISO64524E-04 g
Flame Rating0.8mmUL94HB
1.5mmUL94HB
FMVSS FlammabilityFMVSS302B