Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC DF-0046P BK8782 SABIC INNOVATIVE US
LNP™ THERMOCOMP™
Plastic bag、Electrical appliances
Easy to demould、Easy to form
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | SABIC INNOVATIVE US/DF-0046P BK8782 |
---|---|---|---|
1.8MPa, Unannealed,64.0mm Span | ISO75-2/Af | 138 °C | |
1.8MPa, Unannealed,3.20mm | ASTMD648 | 137 °C | |
Flow:-40 to 40°C | ISO11359-2 | 7E-05 cm/cm/°C | |
0.45MPa, Unannealed,3.20mm | ASTMD648 | 141 °C | |
Flow:-40 to 40°C | ASTME831 | 1.1E-04 cm/cm/°C |
Physical | Test Condition | Test Method | SABIC INNOVATIVE US/DF-0046P BK8782 |
---|---|---|---|
Equilibrium,23°C,50%RH | ISO62 | 0.10 % | |
Modeling Shrinkage | TD:24小时 | ASTMD955 | 0.30到0.50 % |
ASTMD570 | 0.40 % | ||
Modeling Shrinkage | MD:24小时 | ASTMD955 | 0.20到0.40 % |
Mechanical Properties | Test Condition | Test Method | SABIC INNOVATIVE US/DF-0046P BK8782 |
---|---|---|---|
ASTMD638 | 6160 Mpa | ||
fracture | ASTMD638 | 95.1 Mpa | |
ISO527-2 | 97.0 Mpa | ||
ISO527-2 | 3.3 % | ||
ASTMD638 | 3.6 % |
Impact Properties | Test Condition | Test Method | SABIC INNOVATIVE US/DF-0046P BK8782 |
---|---|---|---|
ASTMD256 | 75 J/m | ||
ISO180/1A | 8.2 kJ/m² | ||
Unnotched Izod Impact Strength | 23°C | ASTMD4812 | 470 J/m |
Instrumented Dart Impact | 23°C,EnergyatPeakLoad | ASTMD3763 | 10.5 J |
Flammability | Test Condition | Test Method | SABIC INNOVATIVE US/DF-0046P BK8782 |
---|---|---|---|
Flame Rating | 1.50mm,TestingbySABIC | UL94 | V-0 |