Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PET TechnoPet GF 20 2 0 TECHNOCOMPOUND GERMANY
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Impact resistance | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoPet GF 20 2 0 |
---|---|---|---|
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 8.0 kJ/m² |
-30°C | ISO 179/1eA | 8.0 kJ/m² | |
Impact strength of simply supported beam without notch | 23°C | ISO 179/1eU | 25 kJ/m² |
-30°C | ISO 179/1eU | 25 kJ/m² |
hardness | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoPet GF 20 2 0 |
---|---|---|---|
ball-indentation hardness | ISO 2039-1 | 230 MPa |
Electrical performance | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoPet GF 20 2 0 |
---|---|---|---|
Volume resistivity | IEC 60093 | >1.0E+16 ohms·cm | |
relative permittivity | 100Hz | IEC 60250 | 4.60 |
dielectric strength | 1.00mm | IEC 60243-1 | 31 kV/mm |
relative permittivity | 1MHz | IEC 60250 | 4.10 |
Compared to the Leakage Tracking Index (CTI) | 解决方案A | IEC 60112 | PLC 2 |
Surface Resistivity | IEC 60093 | >1.0E+14 ohms |
Mechanical properties | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoPet GF 20 2 0 |
---|---|---|---|
tensile strength | 断裂 | ISO 527-2/5 | 130 MPa |
Tensile strain | 断裂 | ISO 527-2/5 | 2.0 % |
Tensile modulus | ISO 527-2/1 | 8000 MPa |
flammability | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoPet GF 20 2 0 |
---|---|---|---|
UL flame retardant rating | 0.8mm | UL 94 | HB |
Burning wire flammability index | 2.0mm | IEC 60695-2-12 | 750 °C |
physical property | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoPet GF 20 2 0 |
---|---|---|---|
Shrinkage rate | TD | ISO 2577 | 1.1 % |
Water absorption rate | 23°C,24hr | ISO 62 | 0.20 % |
Shrinkage rate | MD | ISO 2577 | 0.30 % |
Water absorption rate | 饱和,23°C | ISO 62 | 0.45 % |
density | ISO 1183 | 1.51 g/cm³ | |
Viscosity value | 降低的粘度 | ISO 1628 | 66.0 ml/g |
Thermal performance | Test Condition | Test Method | TECHNOCOMPOUND GERMANY/TechnoPet GF 20 2 0 |
---|---|---|---|
melting temperature | ISO 11357-3 | 240 °C | |
vicat | ISO 306/B50 | 250 °C | |
Heat distortion temperature | 1.8MPa,未退火,HDT | ISO 75-2/A | 215 °C |
Linear coefficient of thermal expansion | MD:23到80°C | ISO 11359-2 | 3E-05 cm/cm/°C |
Heat distortion temperature | 8.0MPa,未退火,HDT | ISO 75-2/C | 75.0 °C |