Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

EMA Optema™ TC 110 Cast ExxonMobil
--
ExxonMobil, ExxonMobil Chemical in the United States
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| thermal performance | Test Condition | Test Method | ExxonMobil/Optema™ TC 110 Cast |
|---|---|---|---|
| Vicat softening temperature | ASTM D1525 | 53.0 °C |
| film | Test Condition | Test Method | ExxonMobil/Optema™ TC 110 Cast |
|---|---|---|---|
| Dart impact | ASTM D1709A | 220 g | |
| Elmendorf tear strength | MD | ASTM D1922 | 22 g |
| TD | ASTM D1922 | 360 g | |
| elongation | Break | ASTM D882 | 360 % |
| Secant modulus | ASTM D882 | 50.8 MPa | |
| Tensile strain | Break | ASTM D882 | 810 % |
| tensile strength | Break | ASTM D882 | 23.5 MPa |
| Break,TD | ASTM D882 | 17.1 MPa |
| Physical properties | Test Condition | Test Method | ExxonMobil/Optema™ TC 110 Cast |
|---|---|---|---|
| melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 2.0 g/10min |
| Methacrylic acid content | ExxonMobilMethod | 21.5 wt% |
| optical performance | Test Condition | Test Method | ExxonMobil/Optema™ TC 110 Cast |
|---|---|---|---|
| gloss | 45° | ASTM D2457 | 34 |
| turbidity | ASTM D1003 | 18 % |