TPU 58887 NOVEON USA
ESTANE®
composite、Masterbatch
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
hardness | Test Condition | Test Method | NOVEON USA/58887 |
---|---|---|---|
邵氏A,5秒 | ASTMD2240 | 84到90 |
Mechanical properties | Test Condition | Test Method | NOVEON USA/58887 |
---|---|---|---|
1000Cycles,1000g,H-18转轮 | ASTMD3389 | 40.0 mg |
optical performance | Test Condition | Test Method | NOVEON USA/58887 |
---|---|---|---|
Haze ratio | ASTMD1003 | 1.0 % |
aging | Test Condition | Test Method | NOVEON USA/58887 |
---|---|---|---|
volume change | 23°C,24hr,在水中 | ASTMD471 | 1.1 % |
elastomer | Test Condition | Test Method | NOVEON USA/58887 |
---|---|---|---|
Tensile stress | 100%应变,0.762mm | ASTMD412 | 6.90 Mpa |
300%应变,0.762mm | ASTMD412 | 12.4 Mpa | |
tear strength | 开裂 | ASTMD470 | 26 kN/m |
0.762mm2 | ASTMD624 | 87.3 kN/m | |
elongation | 断裂,0.762mm | ASTMD412 | 500 % |
Stretch permanent deformation | 200%应变 | ASTMD412 | 18 % |
tensile strength | 断裂,0.762mm | ASTMD412 | 51.7 Mpa |
Thermal performance | Test Condition | Test Method | NOVEON USA/58887 |
---|---|---|---|
Kofler Melting Temperature | 内部方法 | 150 °C | |
Glass Transition Temperature | DSC | -45.0 °C | |
melting temperature | DSC | 140 °C |