Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

PC 923 WH SABIC INNOVATIVE US
LEXAN™
Communication equipment
High rigidity、Weather resistance
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | SABIC INNOVATIVE US/923 WH |
---|---|---|---|
Heat Deflection Temperature | 1.8MPa,未退火,6.40mm | ASTMD648 | 132 °C |
RTIElec | UL746 | 130 °C | |
Vicat Softening Temperature | ASTMD15256 | 152 °C | |
RTI | UL746 | 130 °C | |
Thermal Conductivity | ASTMC177 | 0.19 W/m/K | |
Linear thermal expansion coefficient | MD:-40到95°C | ASTME831 | 6.8E-05 cm/cm/°C |
Evolution Calendar intelligent importer | UL746 | 120 °C | |
Heat Deflection Temperature | 0.45MPa,未退火,6.40mm | ASTMD648 | 138 °C |
Hardness | Test Condition | Test Method | SABIC INNOVATIVE US/923 WH |
---|---|---|---|
Rockwell Hardness | M级 | ASTMD785 | 70 |
R级 | ASTMD785 | 118 |
Mechanical Properties | Test Condition | Test Method | SABIC INNOVATIVE US/923 WH |
---|---|---|---|
Flexural Modulus | 50.0mm跨距 | ASTMD790 | 2240 Mpa |
Flexural Strength | 屈服,50.0mm跨距 | ASTMD790 | 91.0 Mpa |
Tensile Elongation | 屈服 | ASTMD638 | 7.0 % |
断裂 | ASTMD638 | 90 % | |
Tensile Strength | 屈服 | ASTMD638 | 62.1 Mpa |
断裂 | ASTMD638 | 55.8 Mpa | |
Taber Abrasion Resistance | 1000Cycles,1000g,CS-17转轮 | ASTMD1044 | 10.0 mg |
Physical | Test Condition | Test Method | SABIC INNOVATIVE US/923 WH |
---|---|---|---|
Moisture Absorption | 24hr | ASTMD570 | 0.15 % |
Outdoor Suitability | UL746C | f1 | |
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.50到0.70 % |
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 15 g/10min |
Moisture Absorption | 平衡,23°C | ASTMD570 | 0.35 % |
Specific Volume | ASTMD792 | 0.835 cm³/g | |
Density / Specific Gravity | -- | ASTMD792 | 1.22 g/cm³ |
Moisture Absorption | 平衡,100°C | ASTMD570 | 0.58 % |
Impact Properties | Test Condition | Test Method | SABIC INNOVATIVE US/923 WH |
---|---|---|---|
Notched Izod Impact Strength | 23°C | ASTMD256 | 640 J/m |
Gardner Impact | 23°C | ASTMD3029 | 169 J |
Tensile Impact Strength | ASTMD1822 | 525 kJ/m² | |
Unnotched Izod Impact Strength | 23°C | ASTMD4812 | 3200 J/m |
Flammability | Test Condition | Test Method | SABIC INNOVATIVE US/923 WH |
---|---|---|---|
Flame Rating | 1.47mm | UL94 | V-0 |
Oxygen Index | ASTMD2863 | 35 % |
Electrical Properties | Test Condition | Test Method | SABIC INNOVATIVE US/923 WH |
---|---|---|---|
Dielectric Constant | 60Hz | ASTMD150 | 3.01 |
50Hz | ASTMD150 | 3.01 | |
Dissipation Factor? | 50Hz | ASTMD150 | 9E-04 |
60Hz | ASTMD150 | 9E-04 | |
1MHz | ASTMD150 | 0.010 | |
Arc Resistance | ASTMD495 | PLC7 | |
Dielectric Constant | 1MHz | ASTMD150 | 2.96 |
Comparative Tracking Index | CTI | UL746 | PLC 3 |
High Amp Arc Ignition | HAI | UL746 | PLC 2 |
Volume Resistivity | ASTMD257 | >1.0E+17 ohms·cm | |
Hot-wire Ignition | HWI | UL746 | PLC 1 |
High Voltage Arc Tracking Rate | HVTR | UL746 | PLC 3 |
Dielectric Strength | 3.20mm,inAir | ASTMD149 | 17 KV/mm |