Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

HDPE HIDEN® P300X YUHWA Korea Petrochemical Ind. Co., Ltd.
--
Pipeline system
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Supplementary Information | Test Condition | Test Method | YUHWA Korea Petrochemical Ind. Co., Ltd./HIDEN® P300X |
|---|---|---|---|
| Crosslinking degree | ISO 15875 | >75 % |
| thermal performance | Test Condition | Test Method | YUHWA Korea Petrochemical Ind. Co., Ltd./HIDEN® P300X |
|---|---|---|---|
| Brittle temperature | ASTM D746 | <-80.0 °C | |
| Vicat softening temperature | ASTM D1525 | 124 °C |
| mechanical properties | Test Condition | Test Method | YUHWA Korea Petrochemical Ind. Co., Ltd./HIDEN® P300X |
|---|---|---|---|
| elongation | Break | ASTM D638 | >500 % |
| tensile strength | Yield | ASTM D638 | 24.5 MPa |
| Physical properties | Test Condition | Test Method | YUHWA Korea Petrochemical Ind. Co., Ltd./HIDEN® P300X |
|---|---|---|---|
| density | ASTM D1505 | 0.948 g/cm³ | |
| Environmental stress cracking resistance | ASTM D1693B | >5000 hr | |
| melt mass-flow rate | 190°C/2.16kg | ASTM D1238 | 0.030 g/10min |
| Water absorption rate | Equilibrium | ASTM D570 | <0.010 % |
| impact performance | Test Condition | Test Method | YUHWA Korea Petrochemical Ind. Co., Ltd./HIDEN® P300X |
|---|---|---|---|
| Impact strength of cantilever beam gap | ASTM D256 | 无断裂 |