Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PA6/66 C40 LN BASF GERMANY
Ultramid® 
film
high viscosity
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

PhysicalTest ConditionTest MethodBASF GERMANY/C40 LN
Modeling ShrinkageMD  MDASTM D9550.70 到 1.2 %
DensityASTM D7921.36 g/cm³
Melt Mass-Flow Rate230℃,2.16kgASTM D12389 g/10min
Mechanical PropertiesTest ConditionTest MethodBASF GERMANY/C40 LN
Flexural Strength断裂  断裂 3ASTM D79045 Mpa
Tensile Strength屈服  屈服 2ASTM D63820 Mpa
Rockwell HardnessR 级  ASTM D785105
Flexural ModulusASTM D7903000 Mpa
Tensile Strain断裂  断裂 2ASTM D63840 %
ThermalTest ConditionTest MethodBASF GERMANY/C40 LN
Heat Deflection Temperature1.8 MPa,未退火  ASTM D64868 °C
Vicat Softening TemperatureASTM D1525 4110 °C
Impact PropertiesTest ConditionTest MethodBASF GERMANY/C40 LN
Notched Izod Impact Strength23℃,3.2mm  ASTM D25625 J/m

Contact Us

Get App

Top