Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
EVA LD-755 EXXONMOBIL USA
Escorene™ Ultra 
Hot melt adhesive、adhesive
No opening agent
TDS
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodEXXONMOBIL USA/LD-755
Dart impact-40°CASTM D376325.8 J
23°CASTM D376314.9 J
hardnessTest ConditionTest MethodEXXONMOBIL USA/LD-755
Shore hardness邵氏A,15秒ASTM D224070
邵氏D,15秒ASTM D224019
Mechanical propertiesTest ConditionTest MethodEXXONMOBIL USA/LD-755
Flexural modulus1%正割ASTM D79018.5 Mpa
elongation断裂ASTM D638>800 %
tensile strength 断裂ASTM D6384.83 Mpa
physical property Test ConditionTest MethodEXXONMOBIL USA/LD-755
Vinyl acetate contentASTM D-256-9727.6 wt%
melt mass-flow rate190°C/2.16kgASTM D123825 g/10min

Contact Us

Get App

Top