Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

TPU T370A-3 LUBRIZOL USA
ESTANE®
Electrical applications
Chemical resistance,wear resistant
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | LUBRIZOL USA/T370A-3 |
---|---|---|---|
Vicat softening temperature | ASTM D-1525 | 70 °C |
mechanical properties | Test Condition | Test Method | LUBRIZOL USA/T370A-3 |
---|---|---|---|
elongation | Break | 900 % | |
Permanent compression deformation | 23℃,22.0hr | ASTM D-395 | 10 % |
tear strength | ASTM D-624 | 68.6 kN/m | |
tensile strength | 100%Strain | ASTM D-412 | 3.14 Mpa |
300%Strain | MPa | ||
Yield | MPa |
Physical properties | Test Condition | Test Method | LUBRIZOL USA/T370A-3 |
---|---|---|---|
Shore hardness | ShoreA | ASTM D-2240 | 75 |
Shrinkage rate | MD | ASTM D-955 | 0.6 % |