Material Comparison

Product Info
Product Name
Brand Name
Usages
Properties
Certificates
PPO(PPE) TYNELOY® NAV210 TYNE USA
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodTYNE USA/TYNELOY® NAV210
Impact strength of cantilever beam gap6.35mmASTM D256210 J/m
hardnessTest ConditionTest MethodTYNE USA/TYNELOY® NAV210
Rockwell hardnessR级ASTM D785115
Mechanical propertiesTest ConditionTest MethodTYNE USA/TYNELOY® NAV210
elongation断裂ASTM D63840 %
Flexural modulusASTM D7902480 MPa
tensile strength 屈服ASTM D63852.4 MPa
bending strengthASTM D79086.9 MPa
flammabilityTest ConditionTest MethodTYNE USA/TYNELOY® NAV210
UL flame retardant rating3.2mmUL 94V-0
1.6mmUL 94V-1
physical property Test ConditionTest MethodTYNE USA/TYNELOY® NAV210
Water absorption rate24hrASTM D5700.070 %
densityASTM D7921.10 g/cm³
Shrinkage rateMD:3.18mmASTM D9550.50to0.70 %
Thermal performanceTest ConditionTest MethodTYNE USA/TYNELOY® NAV210
Heat distortion temperature1.8MPa,未退火,HDTASTM D64898.9 °C
0.45MPa,未退火,HDTASTM D648110 °C