Material Comparison
Add Comparison Model
Highlight Differences
Hide Same

Product Name / Manufacturer / Model

Brand

Typical Applications

Properties

Color

Form

Processing Methods

Grade

Filler

Recycled Content

Certificates

Reference Price

elastomerTest ConditionTest MethodHUNTSMAN GERMANY/A 60 E 4902
tear strength0.635mmASTM D62435.9 kN/m
tensile strength300%Strain,0.635mmASTM D4124.07 Mpa
tear strength0.635mmDIN 5351525 kN/m
Tensile strainBreak,0.635mmASTM D412720 %
Permanent compression deformation23°C,70hrDIN 5351735 %
tensile strength100%Strain,0.635mmDIN 535041.40 Mpa
300%Strain,0.635mmDIN 535042.40 Mpa
Tensile strainBreak,0.635mmDIN 53504900 %
Permanent compression deformation70°C,24hrASTM D39580 %
23°C,70hrASTM D39540 %
Shore hardnessASTM D263260 %
Permanent compression deformation200%StrainDIN 535048 %
70°C,24hrDIN 5351760 %
tensile strength100%Strain,0.635mmASTM D4122.34 Mpa
Break,0.635mmDIN 5350410.0 Mpa
Permanent compression deformation200%StrainASTM D4128 %
tensile strengthBreak,0.635mmASTM D4127.52 Mpa
mechanical propertiesTest ConditionTest MethodHUNTSMAN GERMANY/A 60 E 4902
Wear resistance--DIN 5351643 mm³
--ASTM D39543 mm³
hardnessTest ConditionTest MethodHUNTSMAN GERMANY/A 60 E 4902
Shore hardnessShoreD,InjectionASTM D224015
ShoreD,InjectionDIN 5350515
ShoreA,InjectionASTM D224056
ShoreA,InjectionDIN 5350555
Physical propertiesTest ConditionTest MethodHUNTSMAN GERMANY/A 60 E 4902
Melt Volume Flow Rate (MVR)160°C/8.7kg35.0 cm3/10min
thermal performanceTest ConditionTest MethodHUNTSMAN GERMANY/A 60 E 4902
TMALow:635.0μmInternal Method110 °C
High:635.0μmInternal Method145 °C
Melting temperatureInternal Method98.9to130 °C