Material Comparison
Add Comparison Model
Select Products for Comparison (1/4)
Highlight Differences
Hide Same
Product Name / Manufacturer / Model
Grade
Reference Price
| thermal performance | Test Condition | Test Method | NATPET SAUDI/HP462S |
|---|---|---|---|
| Vicat softening temperature | -- | ISO 306/B50 | 90.0 °C |
| Hot deformation temperature | 0.45MPa,Unannealed | ISO 75-2/B | 85.0 °C |
| Vicat softening temperature | -- | ISO 306/A50 | 154 °C |
| mechanical properties | Test Condition | Test Method | NATPET SAUDI/HP462S |
| Tensile modulus | ISO 527-2 | 1450 Mpa | |
| Tensile strain | Yield | ISO 527-2 | 8.0 % |
| tensile strength | Yield | ISO 527-2 | 34.0 Mpa |
| Tensile strain | Break | ISO 527-2 | >50 % |
| Physical properties | Test Condition | Test Method | NATPET SAUDI/HP462S |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 36 g/10min |