TPE G3548L DUPONT USA
Hytrel®
Automotive sector、Wire and cable、Electrical appliances、Electronic field、Electrical field
Low temperature resistanc
UL
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Thermal Properties | Test Condition | Test Method | DUPONT USA/G3548L |
---|---|---|---|
Vicat Softening Temperature | ASTM D-1525 | 77 °C | |
Thermal distortion temperature | @0.5Mpa | ASTM D-648 | N/A °C |
@0.18Mpa | ASTM D-648 | N/A °C | |
Melting Temperature | ASTM D-3418 | 156 °C |
Physical | Test Condition | Test Method | DUPONT USA/G3548L |
---|---|---|---|
Taber wear | CS-17轮 | ASTM D-1044 | 30 mg/1000rev |
Melt index | ASTM D-1238 | 10 g/10min | |
Taber wear | H 18轮 | ASTM D-1044 | 310 mg/1000rev |
Moisture Absorption (24hr) | ASTM D-570 | 5 % |
Mechanical Properties | Test Condition | Test Method | DUPONT USA/G3548L |
---|---|---|---|
Durometer Hardness | ASTM D-2240 | 35 | |
Tearing Strength | ASTM D-1004 | 51 kN/m | |
Tensile Elongation (Break) | ASTM D-638 | 200 % | |
Tensile Strength | 5%伸长 | ASTM D-638 | 1.7 Mpa |
Notched Izod Impact Strength | 23℃ | ASTM D-256 | 不破裂 J/m |
Tensile Strength | 10%伸长 | ASTM D-638 | 2.6 Mpa |
Tensile Strength (Break) | ASTM D-638 | 10.3 Mpa | |
Tensile Modulus | 23℃ | ASTM D-790 | 32.4 Mpa |
Other | Test Condition | Test Method | DUPONT USA/G3548L |
---|---|---|---|
Ross Flex | ASTM D-1052 | >1×10 |