PP HBG 429D G82766 LYONDELLBASELL HOLAND
HOSTALEN
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
thermal performance | Test Condition | Test Method | LYONDELLBASELL HOLAND/HBG 429D G82766 |
---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/A | 130 °C |
Vicat softening temperature | ISO 306/B | 130 °C |
mechanical properties | Test Condition | Test Method | LYONDELLBASELL HOLAND/HBG 429D G82766 |
---|---|---|---|
Bending modulus | 23°C | ISO 178/A | 4000 Mpa |
bending strength | 23°C | ISO 178/A | 105 Mpa |
Tensile modulus | 23°C | ISO 527-2 | 4700 Mpa |
Tensile strain | Break | ISO 527-2 | 4.5 % |
tensile strength | Yield,23°C | ISO 527-2 | 75.0 Mpa |
Physical properties | Test Condition | Test Method | LYONDELLBASELL HOLAND/HBG 429D G82766 |
---|---|---|---|
melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 5.0 g/10min |
Melt Volume Flow Rate (MVR) | 230°C/2.16kg | ISO 1133 | 6.00 cm3/10min |
impact performance | Test Condition | Test Method | LYONDELLBASELL HOLAND/HBG 429D G82766 |
---|---|---|---|
Impact strength of simply supported beam without notch | 0°C | ISO 179/1eU | 6.0 kJ/m² |
23°C | ISO 179/1eU | 40 kJ/m² |