Material Comparison
Product Info
Product Name
Brand Name
Usages
Properties
Certificates

ABS+PA Romiloy® 4010/07-1 UV ROMIRA GERMANY
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
Test Condition | Test Method | ROMIRA GERMANY/Romiloy® 4010/07-1 UV | |
---|---|---|---|
UL flame retardant rating | 1.6mm | UL 94 | HB |
Linear coefficient of thermal expansion | MD:20到80°C | ISO 11359-2 | 1.4E-04 cm/cm/°C |
Flexural modulus | 23°C | ISO 178 | 1700 MPa |
Charpy Notched Impact Strength | -30°C | ISO 179/1eA | 19 kJ/m² |
tensile strength | 23°C | ISO 527-2/50 | 43.0 MPa |
Charpy Notched Impact Strength | 23°C | ISO 179/1eA | 72 kJ/m² |
bending strength | 23°C | ISO 178 | 66.0 MPa |
vicat | ISO 306/B50 | 120 °C | |
density | 23°C | ISO 1183 | 1.06 g/cm³ |
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | 无断裂 |
23°C | ISO 179/1eU | 无断裂 | |
Heat distortion temperature | 0.45MPa,未退火,HDT | ISO 75-2/B | 96.0 °C |
Tensile modulus | 23°C | ISO 527-2/1 | 2000 MPa |
melt mass-flow rate | 260°C/5.0kg | ISO 1133 | 32 g/10min |
Tensile strain | 断裂,23°C | ISO 527-2/50 | >100 % |
Shrinkage rate | 23°C | ISO 294-4 | 0.60to0.90 % |
Contact Us
Get App
Top