POM MF3020 KEP KOREA
KEPITAL®
--
Glass fiber reinforced,Ground glass fiber reinfo
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Basic Performance | Test Condition | Test Method | KEP KOREA/MF3020 |
|---|---|---|---|
| melt mass-flow rate | ASTM D-1238 | 18 g/10 min |
| thermal performance | Test Condition | Test Method | KEP KOREA/MF3020 |
|---|---|---|---|
| Combustibility | t0.8mm | UL -94 | HB |
| Hot deformation temperature | 4.6kgf/cm2 | ASTM D-648 | 163 °C |
| 18.6kgf/cm2 | ASTM D-648 | 135 °C | |
| Linear coefficient of thermal expansion | 20℃-80℃ | ASTM D-696 | 9 ×10-5cm/cm/℃ |
| Melting temperature | 10℃/min | DSC Method | 165 °C |
| mechanical properties | Test Condition | Test Method | KEP KOREA/MF3020 |
|---|---|---|---|
| Bending modulus | 23℃ | ASTM D-790 | 4.60 ×104kgf/cm2 |
| ASTM D790/ISO 178 | 566000 kg/cm²(MPa)[Lb/in²] | ||
| bending strength | ASTM D790/ISO 178 | 14500 kg/cm²(MPa)[Lb/in²] | |
| 23℃ | ASTM D-790 | 1.100 Kgf/cm2 | |
| elongation | 23℃ | ASTM D-638 | 4 % |
| Impact strength of cantilever beam gap | Notch t3.2mm | ASTM D-256 | 4.5 Kgf.cm/cm |
| t3.2mm S type | ASTM D-1822 | 50 kgf.cm/cm2 | |
| Rockwell hardness | M scale | ASTM D-785 | M83 |
| Shrinkage rate | t3mm,直径100mm | 1.7 % | |
| Tensile modulus | ASTM D638/ISO 527 | 653000 kg/cm²(MPa)[Lb/in²] | |
| tensile strength | 23℃ | ASTM D-638 | 630 Kgf/cm2 |
| Electrical performance | Test Condition | Test Method | KEP KOREA/MF3020 |
|---|---|---|---|
| Surface resistivity | ASTM D-257 | 1×1016 欧姆 | |
| Volume resistivity | ASTM D-257 | 1×1014 欧姆.cm |
| Physical properties | Test Condition | Test Method | KEP KOREA/MF3020 |
|---|---|---|---|
| density | ASTM D792/ISO 1183 | 1.55 | |
| filler content | 20 % | ||
| Water absorption rate | 23℃,60%RH | ASTM D-570 | 0.20 % |