Certificates

EVA 12-9 BEIJING EASTERN
--
Injection molding
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
Plastic Datasheets
| Basic Performance | Test Condition | Test Method | BEIJING EASTERN/12-9 |
|---|---|---|---|
| density | ASTM D-1505 | 0.932 | |
| melt mass-flow rate | ASTM D-1238 | 9 g/10 |
| thermal performance | Test Condition | Test Method | BEIJING EASTERN/12-9 |
|---|---|---|---|
| Melting temperature | 97 °C | ||
| Vicat softening temperature | ASTM D-1525 | 69 °C |
| mechanical properties | Test Condition | Test Method | BEIJING EASTERN/12-9 |
|---|---|---|---|
| Elongation at Break | TD | ASTM D-6398 | 800 % |
| MD | ASTM D-6398 | 800 % | |
| Shore hardness | D | ASTM D-2240 | 38 |
| A | ASTM D-2240 | 94 | |
| tensile strength | Yield,MD | ASTM D-638 | 5.3 N/mm |
| MD,Break | ASTM D-638 | 10.3 N/mm | |
| Yield,TD | ASTM D-638 | 5.3 N/mm | |
| TD,Break | ASTM D-638 | 10.3 N/mm |
| Electrical performance | Test Condition | Test Method | BEIJING EASTERN/12-9 |
|---|---|---|---|
| Dielectric constant | 2×10 | ASTM D-150 | 2.8 |
| Dielectric strength | ASTM D-149 | 700 KV/cm |
| Physical properties | Test Condition | Test Method | BEIJING EASTERN/12-9 |
|---|---|---|---|
| Vinyl acetate content | ISC.DIS 8965/1989(E) | 12 % |