PP Copolymer Jampilen RP1903 Jam Polypropylene Company
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--
--

Plastic Datasheets

Impact resistanceTest ConditionTest MethodJam Polypropylene Company/Jampilen RP1903
Charpy Notched Impact Strength0°CISO 179/A2.0 kJ/m²
23°CISO 179/A6.0 kJ/m²
hardnessTest ConditionTest MethodJam Polypropylene Company/Jampilen RP1903
ball-indentation hardnessH358/30ISO 2039-158.0 MPa
Mechanical propertiesTest ConditionTest MethodJam Polypropylene Company/Jampilen RP1903
Tensile modulusISO 527-21100 MPa
Tensile strain断裂ISO 527-2>50 %
屈服ISO 527-214 %
tensile strength 屈服ISO 527-230.0 MPa
optical performance Test ConditionTest MethodJam Polypropylene Company/Jampilen RP1903
Haze ratio1000µm,注塑ASTM D10039.0 %
400µm,吹塑ASTM D1003<3.0 %
physical property Test ConditionTest MethodJam Polypropylene Company/Jampilen RP1903
densityISO 11830.900 g/cm³
melt mass-flow rate230°C/2.16kgISO 113311 g/10min
Thermal performanceTest ConditionTest MethodJam Polypropylene Company/Jampilen RP1903
Heat distortion temperature0.45MPa,未退火,HDTISO 75-2/B72.0 °C

Contact Us